PRETREATMENT
A) Seven-tank process is carried out.
B) All the gaps, welding spots, joints are given a coat of
m-seal or equivalent finishing material.
SPRAY PAINTINGS
A) Two coats of red oxide are applied across the complete
structure
B) The Zinc chromate manufacture by reputed companies like
Sigma paints are used (This process is carried out for spray
painting only)
PROCESS TREATMENT
A) The painted structure doors & covers are oven baked.
B) The painted structure is inspected & fault if any are
rectified.
C) Panels are randomly tested as per peel off test.
D) It is verified that the structure is hard & scratch
proof.
E) The thickness of paint is not less than 50-60 microns
approximately
POWDER COATING
After pretreatment the job is baked for about 70-80 degree
centigrade, which enabled to remove the moister contents.
After baking the jobs & again baked for about 200 degree
centigrade to get the required result.
The powder used is of reputed make like Inter phone, Asian
Marpole etc.
= Designing
= Fabrication
= Painting / Powder Coating
= Selection of Bus Bars
= Assembly and Wiring
= Testing of Panels
= Automatic P.F. Control Panels
= Auto Mains Failure Panels
= Motor Control Center Panels
= Power Control Centers Panels
= Synchronizing Panels
= Capacitor Control Panels
= Bus Ducts Up to 6400 A
= Soft Starter Panels
= VHD Panels
= Instrumentation Panels